Gh4033 Nicke Tube Superalloy with Sufficient High Temperature Strength M36

Gh4033 Nicke Tube Superalloy with Sufficient High Temperature Strength M36

Production status of nickel alloy Tube:Hot working condition (R)Cold working condition (Y)Annealing state (M)Nickel Tube
SHARE

Description

Basic Info.
Model NO. GH4033
Process Hot Rolling
Standard 1 Gjb 1953-1994
Diametre 20mm-55mm
Material Nickel Chromium
Surface Acid Wash, Polishing
Grade 1 Gh4033
Transport Package Wooden Case
Specification Customized
Trademark Starship
Origin Shenyang. China
HS Code 7507120000
Production Capacity 4500 Tons Per Year
Product Description
Production status of nickel alloy Tube:Hot working condition (R)Cold working condition (Y)Annealing state (M)Nickel Tube manufacturing process:Hot forgingHot rolledCold rolledAnnealingPicklingProduct Description

GH4033 is a superalloy, based on nickel-chromium, adding aluminum, titanium forming'phase diffusion reinforced alloy, with sufficient high temperature strength between 700 and 750ºC, and with good oxidation resistance below 900ºC.The alloy has good hot and cold processing performance, mainly supplying hot rolled rod and billet material, applied to engine rotor parts.

Process performance editing and broadcast

1. The alloy has good thermal processing performance, with forging heating temperature of 1140ºC and final forging of 950ºC.

2. The average grain grain size of the alloy is closely related to the deformation degree and the final forging temperature of the forging.

3. The alloy can be subjected to argon arc welding in the solid dissolution state, and the welding shall be treated in time to eliminate the welding stress.

4. Surface treatment process: mechanical parts shall be electropolished. If mechanical polishing is used, the final polishing mark shall be in the same direction as the blade length.

5. The heating speed of the parts should not be too fast, so the step heating curve can be adopted.Application:this alloy has been used in the manufacture of aero-engine turbine blades, turbine disks and other high temperature bearing componentsPorducts Show:Chemical Elements

NiCCrTiFeMnSiPSBCe
MaxMaxMaxMaxMaxMaxMaxMaxMaxMax
Banlance0.03~0.0819.0~22.02.40~2.804.000.350.650.0150.0070.0100.010

Other product specifications

Round bar

Diameter 8~45mm

Square bar

The edge length is 8 to 30 m m

Hexagonal bar

Inner diameter diameter 8 to 36 m m

Forged round cake

Diameter not greater than 600mm and height 60 to 150 m m

Wire

The outer diameter is 200~800mm, the inner diameter is 50~600mm, and the height is 60~250mm


Pictures:Certification:Why chose us

* Engaged in import and export trade for twenty years* Products are exported to more than 30 countries and regions at home and abroad* Company with greatcredit and multiple sets of machinery and equipment* Competitive price, strict quality control system and on-time delivery* We have our own factory to facilitate our supply

About us


Shenyang Bona Titanium Technology Co., Ltd is located in Shenyang, China. We are the manufacturer of non-ferrous. We have strong technical force and complete equipment, excellent products, the completed equipment and standardized testing to ensure the reliability of the product quality and stability. Our main products include titanium and titanium alloys, nickel and nickel alloys, zirconium and zirconium alloys, the common products such as rod/bar, plate/sheet, wire, tube/pipe. The others like Tees, fasteners, castings, machining parts, forgings, and also other goods made according to the customer's requirements. We have a large stock of titanium bars, plates, lumps and rolled or forged flat materials. We offer our best price and best service to our customers that from all over the world. Please give both of us an opportunity to cooperate with each other

Our Contact